logo
Wuhan Fengfan International Trade Co.,Ltd. 86-27-85615818 info@fengfan.net
Phoenix Lubricant 460 Teflon Sealing Agent

Phoenix Lubricant 460 Teflon Sealing Agent

  • Highlight

    Phoenix 460 Teflon sealing agent

    ,

    Teflon lubricant for aluminum anodizing

    ,

    460 Teflon sealing agent

  • Type
    Anodizing Processes
  • Item
    Teflon Sealing Agent
  • Use
    Aluminum Anodizing
  • Temperature
    10 ~ 40°C
  • Place of Origin
    China
  • Brand Name
    FENGFAN
  • Model Number
    Lubricant 460
  • Minimum Order Quantity
    Negotiable
  • Price
    Negotiable
  • Packaging Details
    Standard export packaging
  • Delivery Time
    15-25 work days
  • Payment Terms
    L/C,D/A,D/P,T/T,Western Union,
  • Supply Ability
    200000pcs/day

Phoenix Lubricant 460 Teflon Sealing Agent

Phoenix Lubricant 460 Teflon Sealing Agent

PRODUCT DESCRIPTION

Phoenix Lubricant 460 sealing agent, containing Teflon PTFE microparticles, can be used as sealing agent for general and hard aluminum anodizing, it can provide a colorless and stable lubricity protective film layer.

ADVANTAGES

  • PTFE, polytetrafluoroethylene, with an excellent corrosion resistance
  • PTFE particles, which can form rubber particles after activation reaction, after soaking, it can be electrostatically adsorbed to the surface of the product to achieve self-lubricating sealing performance
  • After drying, a uniform, colorless and stable protective layer can be obtained
  • Depending on the base material and the concentration of Phoenix Lubricant 460 used, the coefficient of friction can be reduced to approximately 0.11-0.13.

OPERATING CONDITIONS

Item Work conditions
Phoenix Lubricant 460 Immersion 0.5-10 %
Temperature 10 ~ 40°C
Time(about) 20 ~ 120seconds
pH range 8-10(It can be adjusted with ammonia solution or Phoenix Lubricant 460 if necessary)
Agitation No need
Rinsing After process, it can be rinsing or dried directly, depending on the product
Tank material SUS or PP or PVC
Cycle filtration No need
Heating/cooling No need
Exhaust No need
Notes Make sure the 460 is not frozen.